Abstract

A study was conducted on the preservative treatment of Acacia mangium poles to determine the treatment schedule for outdoor use. The poles contained 52.27% sapwood which is generally perishable by wood destroying organisms. In this study, 27 poles were treated with aqueous solution of 10% CCB by Lowry empty cell process. Three different pressures and three time periods were applied to evaluate the depth of penetration and amount of retention of the preservative chemicals. It was observed that preservative chemicals penetrated the entire sapwood portions of the poles which are the main criteria for the protection of poles. But, on the other hand, no significant increase was observed in penetration with the simultaneous increase of pressure and time period, although the retention of the preservatives was found to increase significantly. The highest retention of 22.98 kg/m3 and full penetration of sapwood was observed after 1.04 N/mm2   pressure for three hours. It is expected that the applied pressure and time period are adequate for protecting the Acacia mangium poles from wood destroying organisms in outdoor condition.

Keywords

CCB (Copper-Chrome-Boron), Pressure Process, Penetration, Retention, Preservative Chemicals

Access Options

250/-

Buy Full Access in HTML Format

Instant access to the full article.

References

1. Anon. (1988). Code of  Practice for Preservation of Timber. Bangladesh Standards and Testing Institution. BDS.819:1975, Dhaka:36pp

2. Anon. (1988). Standards for wood poles, Rural Electrification Board, Publication 460, 49pp

3. Anon. (1991). American Wood Preservation Association Standards. AWPA, USA

4. Anon. (1979). Bangladesh Standard Specification for wood poles for overhead power and telecommunication lines. BDS 809:1973:27pp

5. Anon. (1983). Mangium and other Fast-growing Acacias for the Humid Tropics. National Academy Press, Washington, D.C. USA

6. Du Toit, C.B. and Conradie,W.E. (1988). Preservative retention requirements based on sapwood volume for E. qrandis and Eclocziana. Sep. 1988. ( R20 & GST).

7. Elias, G.N.M., Kabir, M.F., Satter, M.A., Lahiry, A.K.  and Bhattacharje, D.K. (1993). Preservative treatment of Acacia mangium, J. Tim Assoc. (India). Vol. xxxix No. 3

8. Goodell, B. and Pendlebury, A.J. (1991). Preservative treatment and field test monitoring of spruce pole stock;Pressure and diffusible chemical treatments. Forest Products Research Society, 1991. Forest Product Journal. 41(4):39-44

Google Scholar

9. Greaves, H. (1985). CCA treated timber facts, figures and comments on health and safety in uses. Forest products newsletter, New series No.-1 CSIRO Division of chemical and wood technology, melbourne

10. Hunt, G.M. and Garrat, G.A. (1967). Wood Preservation. Mcgraw-Hill Book Company Inc. New York. USA.  417pp

11. Kader, R.A. and Kuo, H.S. (1991). Properties of particleboards manufactured from fast growing plantation species In: Recent development in tree plantations of  Humid/Sub-humid tropics of Asia, (eds) Sheikh Ali Abood et al.; 645-691. Proc of a Reg. Sympos. June 5-9, 1989 in Serdang, Malaysia. University Pertanian Malaysia.

Google Scholar

12. Lahiry, A.K. (1996). Adequate preservative treatment of kiln dried Eucalyptus camaldulensis and Acacia mangium for tropical and subtropical wood poles. International Research Group on Wood Preservation (IRG), Section 4. (Processes). Doc, IRG/WP 96-40075:1-10

Google Scholar

13. Latif, M.A. Younus-uzzaman, M. and De, B.C. (1981). Pressure treatment of sundri poles with oil-borne preservative. Bano biggyan patrika. 10 (1&2):41-48. Bangladesh Forest Research Institute, Chittagong

14. National Research Council. (1983). Mangium and other fast growing acacias for the humid tropics. Washington, D.C. National Academy Press. USA

Google Scholar

15. Nishimoto, K. (1982). Toxicity of wood preservatives, In: Mokuzai Hozongaku (Wood Preservative Science) Bunkyou-syuppan, Osaka, Japan 141 pp. (in Japanese)

16. Peylo, A. and Willeitner, H. (1998). Five years leaching of Boron. Section 3. Wood Protecting Chemicals.  Proc. of 30th Annual meeting, International Research Group on Wood Preservation Germany

Google Scholar

17. Sattar, M.A., Kabir, M.F. and Bhattacharjee, D.K. (1993). Physical Mechanical and Seasoning Properties of Acacia mangium and Acacia auriculiformis, Bull. 15, Timber Physics Series, Bangladesh Forest Research Institute, Chittagong

Google Scholar

18. Wang, W.C., Ho, K.S. and Wong, C.N. (1988). Acacia mangium from sabah for plywood and decorative panel manufacture trials. J. Trop. For. Sci. 1(1):42-50

Google Scholar

19. Younus-uzzaman, M. and  Akhter, K. (1999). Pressure treatment of Eucalyptus camaldulensis poles with oil-borne preservative. Bangladesh Journal of Forest science. 28(1): 47-53

Google Scholar

20. Zashimuddin, M., Latif, M.A., Khan, S.A. and Davidson, J. (1983). Performance of different provenances of  Acacia mangium in Bangladesh. Bano Bigg Patrika. 12(1&2):57-61

Google Scholar

About this article

How to cite

Akhter, K. and Chowdhury, M.H., 2015. CCB Preservative Treatment of Acacia mangium Poles by Pressure Process. Journal of Non-Timber Forest Products, 22(2), pp.75-78. https://doi.org/10.54207/bsmps2000-2015-G0BE2V

Publication History

Manuscript Published on 01 June 2015

Share this article

Anyone you share the following link with will be able to read this content: